Research Projects
                                    51 - Fatigue Resistance of Weld  Repaired Ductile Iron Castings
                                    Abstract:
Sometimes casting suppliers find that a casting has imperfections, such as pores, in an...
                                
                                
                            
                                    50 - Tracking Chemistry of Minor  Elements - DIS Foundry Member Survey
                                    Abstract:
In the fall of 2012, a foundry member asked if we could survey members to see if people...
                                
                                
                            
                                    49 - Analysis of Pearlitic Ductile Iron with Enhanced Mechanical Properties
                                    Abstract:
The combination of strength and ductility has been difficult to achieve in the...
                                
                                
                            
                                    48 - Normalizing Heat Treatments to Develop Improved Properties in Heavy Section Iron
                                    Abstract:
The combination of strength and ductility has been difficult to achieve in the...
                                
                                
                            
                                    47 - Literature Summary - Deteriorated Graphite in Casting Surfaces
                                    Abstract:
DIS Research has shown that a considerable drop in the fatigue life of ductile iron...
                                
                                
                            
                                    46 - Optimizing Structure-Property Relationships in Ductile Iron
                                    Abstract:
The purpose of this research study was to identify ways to achieve a higher combination...
                                
                                
                            
                                    45 - Graphite Shape Degradation at the Surface of Chemically Bonded Sand Molds and Cores
                                    Abstract:
Standard specifications of ductile irons are all based on machined test bars either...
                                
                                
                            
                                    44 - Effect of Surface Defects on Fatigue Properties of Ferritic Ductile Iron
                                    Abstract:
The fatigue strength of ferritic ductile iron, Grade EN-GJS-400-18U-LT, was determined...
                                
                                
                            
                                    43 - Dimensional Growth of Ductile Iron Castings During Heat Treatment
                                    Abstract:
The dimensional changes upon heat treatment were studied in three grades of ductile...
                                
                                
                            
                                    42 - Nodularity in Coupons
                                    Abstract:
A correlation between nodularity and ultrasonic velocity was developed for test...
                                
                                
                            
                                    40 - Survey of Greensand Properties of Member Foundries
                                    Abstract:
The sand tests were done in one laboratory known to have many years of expertise in...
                                
                                
                            
                                    39 - Elimination and Neutralization of Boron in Ductile Irons
                                    Abstract: